CuSn6P Welding Wire
1. Physical And Mechanical Properties
(1). Solidus: 910℃
(2). Liquidus: 1040℃
(3). Denseness: 8.7kg/dm³
(4). Elongation: 20%~50
(5). Brinell hardness: 80~90HB
(6). Tensile Strength: 320~360N/mm²
2. Application
CuSn6P Welding Wire is suitable for copper and tin bronze welding, especially for brazing joints of brass and steel, and for repairing copper alloy castings. Our company's tin bronze weld wire has many specifications, including CuSn6P, CuSn9P, CuSn12P and CuSn10.
3. Attention
(1). CuSn6P Welding Wire requires preheating when welding large thick parts.
(2). CuSn6P Welding Wire uses pulsed argon arc welding for multi-layer welding of steel.
(3). If you want to know more about the product, please contact us in time. We sincerely look forward to communicating with you.
4.Chemical Ingredient
Executive Standard |
Classified Code |
Alloy No. |
Cu |
Al |
Fe |
Mn |
Ni |
P |
Pb |
Si |
Sn |
Zn |
Total Other Elements |
ISO24373 |
Cu5180 |
CuSn5P |
bal. |
0.01 |
- |
- |
- |
0.1-0.4 |
0.02 |
- |
4.0-6.0 |
- |
0.5 |
GB/T9460 |
SCu5180 |
CuSn5P |
bal. |
max0.01 |
- |
- |
- |
0.1-0.4 |
max0.02 |
- |
4.0-6.0 |
- |
max 0.5 |
ISO24373 |
Cu5180A |
CuSn6P |
bal. |
0.01 |
0.1 |
- |
- |
0.1-0.4 |
0.02 |
- |
4.0-7.0 |
0.1 |
0.2 |
GB/T9460 |
SCu5180A |
CuSn6P |
bal. |
max0.01 |
max 0.1 |
- |
- |
0.1-0.4 |
max0.02 |
- |
4.0-7.0 |
max 0.1 |
max 0.2 |
BS EN14640 |
Cu5180 |
CuSn6P |
bal. |
0.01 |
0.1 |
- |
- |
0.1-0.4 |
0.02 |
- |
4.0-7.0 |
0.1 |
0.4 |
AWS A5.7 |
C51800 |
ERCuSn-A |
bal. |
0.01 |
- |
- |
- |
0.10-0.35 |
0.02 |
- |
4.0-6.0 |
- |
0.5 |
DIN 1733 |
2.1022 |
SG-CuSn6 |
bal. |
max0.01 |
max 0.1 |
- |
- |
0.10-0.35 |
max0.02 |
- |
5.0-8.0 |
max 0.1 |
max 0.4 |