CuAl9Ni5 Welding Wire
1. Application
CuAl9Ni5 is widely used in marine propellers, turbine parts, valves, screens, pumps, and piping systems. It has a particularly strong resistance to seawater erosion.If you need anything, please contact us.
2. Physical And Mechanical Properties
(1). Solidus: 1015℃
(2). Liquidus: 1045℃
(3). Denseness: 7.5kg/dm³
(4). Elongation: 10%
(5). Brinell hardness: 150~170HB
(6). Tensile Strength: 450~560N/mm²
3.Chemical Ingredient
Executive Standard |
Classified Code |
Alloy No. |
Cu |
Al |
Fe |
Mn |
Ni |
P |
Pb |
Si |
Sn |
Zn |
Total Other Elements |
ISO24373 |
Cu6328 |
CuAl9Ni5Fe3Mn2 |
bal. |
8.5-9.5 |
3.0-5.0 |
0.6-3.5 |
4.0-5.5 |
- |
0.02 |
0.1 |
- |
0.1 |
0.5 |
GB/T9460 |
SCu6328 |
CuAl9Ni5Fe3Mn2 |
bal. |
8.5-9.5 |
3.0-5.0 |
0.6-3.5 |
4.0-5.5 |
- |
max 0.02 |
max 0.1 |
- |
max 0.1 |
max 0.5 |
BS EN14640 |
Cu6328 |
CuAl9Ni5 |
bal. |
8.5-9.5 |
3.0-5.0 |
0.6-3.5 |
4.0-6.0 |
- |
0.02 |
0.2 |
- |
0.1 |
0.4 |
AWS A5.7 |
C63280 |
ERCuNiAl |
bal. |
8.50-9.50 |
3.0-5.0 |
0.60-3.50 |
4.0-5.5 |
- |
0.02 |
0.10 |
- |
0.1 |
0.50 |
DIN 1733 |
2.0923 |
SG-CuAl8Ni6 |
bal. |
8.5-9.5 |
3.0-4.0 |
1.0-2.0 |
4.0-6.0 |
- |
max 0.02 |
max 0.2 |
- |
max 0.1 |
max 0.4 |