Substrate
coating
Titanium strip ASTM B265 Gr1orGr2
Mixed metal oxide
Maximum current density at the anode interface
WA limit value
110 mA/m2
Short-term limit
220 mA/m2
Thermal expansion coefficient
8.7 ×10-5/k
Thermal conductivity(20℃)
15.6 W/(m·K)
Resistivity
0.000056 ohm/cm
Model
Weight
CF-MMO
6.35±0.30mm×0.635±0.07mm×152m±1m